Misplaced Pages

Saturated-surface-dry

Article snapshot taken from[REDACTED] with creative commons attribution-sharealike license. Give it a read and then ask your questions in the chat. We can research this topic together.
Aggregate or porous solid condition

Saturated surface dry (SSD) is defined as the condition of an aggregate in which the surfaces of the particles are "dry" (i.e., surface adsorption would no longer take place), but the inter-particle voids are saturated with water. In this condition aggregates will not affect the free water content of a composite material.

The water adsorption by mass (Am)) is defined in terms of the mass of saturated-surface-dry (Mssd) sample and the mass of oven dried test sample (Mdry) by

A = M s s d M d r y M d r y {\displaystyle A={\frac {M_{ssd}-M_{dry}}{M_{dry}}}}

See also

References

  1. "Aggregate Moisture in Concrete". Concrete Construction. 31 May 2013. Retrieved 2018-11-08.
  2. ftp://ftp.dot.state.tx.us/pub/txdot-info/cst/TMS/400-A_series/pdfs/cnn403.pdf

3- Neville, A. M. “Properties of Concrete”, 4th & Final ed., Longman, Malaysia, 1995 rep. 1996, 844 pp.
4 - Field usage information from a manufacturer - https://blog.kryton.com/2012/08/what-ssd/


Stub icon

This material-related article is a stub. You can help Misplaced Pages by expanding it.

Categories:
Saturated-surface-dry Add topic